TECATRON® PPS CM XP63 BLACK

PPS Compound: 50% fiberglass reinforced material

  Properties ASTM
Test Method
Units Typical Values
Mechanical Tensile Strength D-638 psi 7,500
Tensile Elongation D-638 % @ Break 0.73
Tensile Modulus D-638 psi 1,400,000
Flexural Strength D-790 psi 9,250
Flexural Modulus D-790 psi 1,200,000
Compressive Strength (10%) D-695 psi 17,700
Compressive Strength (1%) D-695 psi 8,500
Compressive Modulus D-695 psi 720,000
Izod Impact Strength (Notched) D-256 ft-lb/in 0.49
Shear Strength D-732 psi -
Hardness D-2240 Shore D 90
Hardness D-785 Rockwell (M) -
Thermal Heat Distortion Temperature D-648 °F 484
Coefficient of Linear
Thermal Expansion
E-831 10-6/°F 32
Thermal Conductivity C-177 BTU in/hr-ft2-°F -
Continuous Use (Mechanical) UL746B ° -
Limiting Oxygen Index D2863 %O2 -
Melt Point DSC °F -
Electrical Dielectric Strength D-149 KVcm -
Dielectric Constant D-150 50Hz, 200°C -
Volume Resistivity D-257 ohm-cm -
Surface Resistivity D-257 ohm/sq -
Physical Specific Gravity D-792 gm/cm3 1.78
Color - - Black
Filler Content - % 50
Water Absorption (RT 24h) D-570 % -
Typical Level of Crystallinity - % -
Other Static Coefficient of Friction D-1894 - -
Kinetic Coefficient of Friction D-1894 - -

Note: Listed properties should be interpreted as typical rather than minimum values. This technical information is presented in good faith and is based upon what is believed to be reliable laboratory data. We cannot guarantee the accuracy or completeness of this information. The responsibility for determining product suitability for any given application lies with the customer.